Geotechnical Characteristics of Benin Formation, Owerri Imo State, Nigeria.

Yazarlar: Akaolisa CCZ, Opara JC, Okechukwu Agbasi

Cilt 3 , Sayı 2 , 2022 , Sayfalar -

Konular:-

DOI:10.36937/ben.2022.4569

Anahtar Kelimeler:Bearing Ratio,Liquid Limit,Linear Shrinkage,Moisture,Plastic Limit

Özet: A good road network consists of a constant stretch of asphalt laid down for a smooth ride. The spot in the smooth ride on the pavement is commonly referred to as "pavement failure." Soil type, load bearing capacity of materials, zone of vulnerability, resistance to permeation, compressibility, shrinkage limit, and other details are frequently required in order to construct a very good and solid foundation for the planned bridge site. In Nigeria, numerous factors contribute to the failure of road construction projects. They are primarily insufficient research on subgrade and other pavement materials (sub-base and base courses) prior to the start of road projects; flawed engineering, including a poor drainage system and supervision throughout road construction; and shoddy workmanship that was superimposed with asphaltic concrete to improve strength. Within the Niger Delta basin, the study area is located between latitude 5.485°N and longitude 7.035°E. The Benin Formation underpins the study area. It is composed primarily of friable sands, conglomerates, very coarse sandstone, and isolated gravel units, as well as intercalation of Pliocene to Miocene shale/clay lenses. Natural Moisture Content (NMC), Linear Shrinkage (LS), Particle Size Distribution, and California Bearing Ratio were among the laboratory tests performed on samples collected at failed and stable sections of some selected road segments (CBR). When compared to the stable sections, the NMC along the failed sections was on the high side (ranging from 13.11 percent to 26.89 percent) (ranging from 11.11 percent to 16.40 percent). The majority of the tested soils passed the 0.075mm sieve with a percentage greater than the Federal Ministry of Works and Housing's maximum of 35% for subgrade materials. The maximum dry density (MDD) for the samples at failed and stable sections was 1550 kg/m3 to 1860 kg/m3; 1650 kg/m3 to 1980 kg/m3; and the Optimum Moisture Content (OMC) was 8.30% to 20.30%. The soaked CBR values ranged from 2 to 17 percent, while the unsoaked values ranged from 4 to 25 percent.


ATIFLAR
Atıf Yapan Eserler
Henüz Atıf Yapılmamıştır

KAYNAK GÖSTER
BibTex
KOPYALA
@article{2022, title={Geotechnical Characteristics of Benin Formation, Owerri Imo State, Nigeria.}, volume={3}, number={0}, publisher={Brilliant Engineering}, author={Akaolisa CCZ,Opara JC,Okechukwu Agbasi}, year={2022} }
APA
KOPYALA
Akaolisa CCZ,Opara JC,Okechukwu Agbasi. (2022). Geotechnical Characteristics of Benin Formation, Owerri Imo State, Nigeria. (Vol. 3). Vol. 3. Brilliant Engineering.
MLA
KOPYALA
Akaolisa CCZ,Opara JC,Okechukwu Agbasi. Geotechnical Characteristics of Benin Formation, Owerri Imo State, Nigeria. no. 0, Brilliant Engineering, 2022.